Brics cromiwm corundum refers to a refractory product made of corundum containing Cr ₂ O3, with the main mineral composition being α - Al ₂ O3- Cr ₂ O3 solid solution, and minor minerals containing a small amount of composite spinel or chromium oxide. It utilizes the characteristic of forming a continuous solid solution between Cr ₂ O3 and Al ₂ O3, and has higher high-temperature performance than pure corundum products. The conventional Cr ₂ O3 content is 9% -15%. Bricks used in the petrochemical industry need to meet the requirements of low silicon, low iron, low alkali, and high purity. This product is divided into two categories: cast and sintered, usually referring to sintered type. Prepare using α - Al ₂ O3 as the main material, add chromium oxide powder, mix and shape it, and then high-temperature burn it, or use grouting method to make the billet. The product has a room temperature compressive strength of>150MPA a dwysedd swmp o fwy na neu'n hafal i 3.0g/cm ³, a gall wrthsefyll cyrydiad o slag metelegol a thoddi gwydr. Defnyddir yn bennaf ar gyfer leinin odynau gwydr, cefnogi ffwrneisi nwyeiddio, ffwrneisi mwyndoddi anfferrus, a briciau athraidd ar gyfer ladlau dur
1. Cyflwyniad:
Brics Corundwm Chromeyn cyfeirio at gynhyrchion anhydrin corundum sy'n cynnwys CR2O3. Ar dymheredd uchel, mae CR2O3 ac Al2O3 yn ffurfio toddiant solet parhaus, gan arwain at berfformiad tymheredd uchel uwch o gynhyrchion cromiwm corundwm o'i gymharu â chynhyrchion corundwm pur. Dylai'r briciau cromiwm corundum a ddefnyddir ar gyfer ffwrneisi nwyeiddio yn y diwydiant petrocemegol fod yn silicon isel, haearn isel, alcali isel, purdeb uchel, a hefyd bod â dwysedd a chryfder uchel. Mae gan y cynhyrchion cromiwm corundwm a ddefnyddir yn helaeth gynnwys CR2O3 yn bennaf o fewn yr ystod o 9% i 15%
2. Cyfansoddiad Mwynau
Y prif gyfansoddiad mwynau yw - toddiant solid Al2O3 -CR2O3. Y cyfansoddiad mwynol eilaidd yw briciau anhydrin gydag ychydig bach o spinel cyfansawdd (neu heb spinel cyfansawdd) a chynnwys cromiwm ocsid o 1% i 30%. Mae dau fath o frics cromiwm corundwm wedi'u hasio a briciau cromiwm sintered corundwm. Yn gyffredinol, mae brics cromiwm corundwm yn cyfeirio at frics cromiwm corundwm sintered
3. CynhyrchuBrics cromiwm corundum
Gan ddefnyddio - Al2O3 fel deunydd crai, gan ychwanegu swm priodol o bowdr cromiwm ocsid a phowdr mân clincer cromiwm corundwm, siapio a thanio ar dymheredd uchel. Mae cynnwys cromiwm ocsid briciau cromiwm corundwm sintered yn gyffredinol is na chynnwys briciau cromiwm corundwm wedi'i asio. Fel arall, gellir defnyddio'r dull castio slyri i baratoi slyri trwchus trwy gymysgu'n unffurf - powdr Al2O3 a phowdr cromiwm ocsid, gan ychwanegu asiantau debonding a rhwymwyr organig, ac ychwanegu rhywfaint o glincer cromiwm corundwm. Gellir gwneud y corff brics trwy ddull growtio ac yna ei danio. Gellir ei ddefnyddio fel leinin ar gyfer odynau gwydr, gorchuddio briciau ar gyfer tyllau llif gwydr wedi'u tynnu, ac fel cefnogaeth ar gyfer dyfeisiau cyn-driniaeth haearn, llosgyddion sbwriel, nwyeiddwyr dan bwysau slyri dŵr glo, ac ati
4. Cais
CymhwysoBrics cromiwm corundumwedi dod yn fwy eang. Un math yw briciau cromiwm corundum a wneir yn bennaf o slag cromiwm metel, a ddefnyddir yn helaeth wrth fwyndoddi sinc ffwrneisi trydan ac odynau anwadaliad. Mae gan frics cromiwm corundwm sefydlogrwydd dirgryniad thermol rhagorol a pherfformiad ymgripiad tymheredd uchel, ac mae hefyd yn cwrdd â gofynion yr economi gylchol genedlaethol.
Defnyddir math arall o frics anhydrin o'r enw spinel cromiwm alwminiwm yn helaeth wrth fwyndoddi copr, gan dorri monopoli briciau cromiwm magnesia mewn un cwymp